Depressed Center Grinding (Type 27) - Aluminum Oxide
PFERD » Grinding & Cut-Off Wheels » Depressed Center Grinding (Type 27) » Aluminum Oxide
Rough grinding wheels manufactured with Aluminum Oxide for grinding ferrous and non-ferrous metals. Available in a variety of styles to match your power tool, work piece material and application.
 |
| A-PS: General Purpose for Steel, Stainless |
General purpose grinding wheel for use on all metals - steel, stainless and non-ferrous. Smooth grinding action and fast removal rates with minimal contact pressure. - Aluminum Oxide grain
- Fast stock removal, good service life
- INOX Rated: Free of iron, sulphur and fillers; suitable for use on stainless steel.
|
|
| |
 |
| A-SG: Long Life for Steel |
High performance grinding wheel provides long service life for reduced wheel changes. Particularly well suited for use in severe, high pressure grinding applications (e.g. edge grinding, beveling, etc). Fast removal rates on carbon steel and all ferrous metals. - Aluminum Oxide grain
- Fast stock removal and long service life
- For steel and all ferrous metals
|
|
| |
 |
| A-SG INOX: Premium Performance - Steel, Stainless |
High performance, long life grinding wheel for stainless steels and high temperature alloys. Smooth grinding action and fast removal rates are achieved with minimal contact pressure. Also suitable for carbon steel and all ferrous metals. - Aluminum Oxide grain
- Fast stock removal and long service life
- INOX Rated: Free of iron, sulphur and fillers; suitable for use on stainless steel.
|
|
| |
 |
| A-SG ALU: For Aluminum and Non-Ferrous Metals |
Non-loading grinding wheels for use on aluminum and all soft, greasy materials susceptible to loading problems. Advanced formulation does not leave a greasy residue on the work piece. Surface can be welded immediately following grinding operation. No secondary surface cleaning operation is necessary. - Aluminum Oxide grain
- Exceptionally fast stock removal combined with soft grinding properties
- Free of paraffin: No cleaning required prior to welding!
|
|
| |
|